Sarlink® TPV is a global brand of thermoplastic vulcanizate, an innovative material with the properties of a rubber that can be processed as a plastic. Sarlink offers time-tested TPV expertise, an extensive product range, superior customer service and fully colorable, high-performance solutions for many complex application challenges.


4000 series  Fully crosslinked EPDM grade


Features: Materials excel in oil resistance, heat resistance and features of rubber.

基本信息
原厂资料
物性表(英文)
产品特性
耐热
耐油
成型方式
注塑
挤出
技术参数
物理性能 值/单位 测试标准 测试条件

密度

0.96 g/cm³ ASTM D792

收缩率

纵向(Flow)

1.7 % Internal
3mm thickness

横向(Across Flow)

1.4 % Internal
3mm thickness
机械性能 值/单位 测试标准 测试条件

拉伸强度

100%延伸率时

6.7 Mpa ASTM D 412
Cross direction

100%延伸率时

7.7 Mpa ASTM D 412
Flow direction

-

14.8 Mpa ASTM D 412
Cross direction

-

13 Mpa ASTM D 412
Flow direction

拉伸延伸率

断裂(brk)

577 % ASTM D 412
Cross direction

断裂(brk)

524 % ASTM D 412
Flow direction

撕裂强度

56 kN/m ASTM D 624
Unnicked, Cross direction

压缩永久形变

59 % ASTM D 395
125℃, 70Hrs

压缩永久形变

39 % ASTM D 395
23℃, 22Hrs

压缩永久形变

40 % ASTM D 395
70℃, 22Hrs
冲击性能 值/单位 测试标准 测试条件

脆化温度

-59 °C ISO 812
硬度性能 值/单位 测试标准 测试条件

邵氏硬度 A

86 A ASTM D 2240
5sec, Extruded sample

邵氏硬度 A

88 A ASTM D 2240
5sec, Injection molded sample
燃烧性能 值/单位 测试标准 测试条件

UL 防火等级

HB

- mm UL94
老化性能 值/单位 测试标准 测试条件

硬度 (热老化)

2 - ASTM D573
Change, 135℃, 1000Hrs

硬度 (热老化)

3 - ASTM D573
Change, 150℃, 168Hrs

拉伸强度(热老化)

92 % ASTM D573
Retention, 135℃, 1000Hrs

拉伸强度(热老化)

90 % ASTM D573
Retention, 150℃, 168Hrs

延伸率(热老化)

84 % ASTM D573
Retention, 135℃, 1000Hrs

延伸率(热老化)

83 % ASTM D573
Retention, 150℃, 168Hrs

体积变化

56 % ASTM D471
ASTM Oil#3, 125℃, 70Hrs