Texin RxS285 resin is an aromatic polyester-based thermoplastic polyurethane. It can be processed by injection molding, extrusion or blow molding.

Texin RxS285 offers outstanding abrasion resistance, impact strength, toughness and flexibility. Typical medical applications include dental ligature, tubing and luers. As with any product, the use of Texin RxS285 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

基本信息
原厂资料
物性表(英文)
产品特性
高冲击
高韧性
耐磨
医疗级
生物相容
电子束灭菌
耐伽马射线
环氧乙烷灭菌(EtO)
法规认证
FDA(食品药品监督管理局)
ISO10993(生物相容性)
成型方式
注塑
挤出
吹塑
技术参数
物理性能 值/单位 测试标准 测试条件

比重

1.202 - ASTM D792

熔体质量流动速率(MFR)

190℃/8.7 kg

4 g/10 min ASTM D 1238

收缩率

纵向(Flow)

0.8 % ASTM D 955
2.54 mm

横向(Across Flow)

0.8 % ASTM D 955
2.54 mm

磨耗

35 mg/1000cy ASTM D 3489
H-18, 1,000-g Load
机械性能 值/单位 测试标准 测试条件

拉伸强度

100%延伸率时

5.34 Mpa ASTM D 412

300%延伸率时

13.1 Mpa ASTM D 412

-

37.9 Mpa ASTM D 412

拉伸延伸率

断裂(brk)

500 % ASTM D 412

弯曲模量

27.6 Mpa ASTM D790
73°F (23°C)

撕裂强度

87.6 kN/m ASTM D 624
Die C

压缩永久形变

35 % ASTM D 395
Postcured, 22 Hours at 158°F (70°C)

压缩永久形变

12 % ASTM D 395
Postcured, 22 Hours at 73°F (23°C)
硬度性能 值/单位 测试标准 测试条件

邵氏硬度 A

85 A ASTM D 2240
热学性能 值/单位 测试标准 测试条件

维卡软化温度(Vicat)

91 °C ASTM D1525
Rate A
其他性能 值/单位 测试标准 测试条件

黄色指数(YI)

15 - ASTM E 313