回到顶部
2024-10-17当前位置:网站首页 > 塑料材料 > TPU(热塑性聚氨酯) >

Texin® 1209

Texin® 1209

Texin® 1209

TPU(热塑性聚氨酯)

科思创 (原拜耳)(Covestro)

产品描述

Texin 1209 resin is an aromatic polyether-based thermoplastic polyurethane; it can be processed by injection molding or extrusion.

Texin 1209 resin is characterized by very good hydrolysis resistance, good low temperature flexibility, resiliency and impact strength, high moisture vapor transmission rates and is plasticizer free. Texin 1209 natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. Applications include soft touch over-molding, roof linings, seals, membranes, films, rigid/flexible composite systems and sport shoe soles. As with any product, use of Texin 1209 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

基本信息
原厂资料
物性表(英文)
产品特性
高冲击
耐低温冲击
食品接触级
无塑化剂(PAEs)
耐水解
法规认证
FDA(食品药品监督管理局)
成型方式
注塑
挤出
技术参数
物理性能 值/单位 测试标准 测试条件

比重

1.07 - ASTM D792

收缩率

纵向(Flow)

0.8 % ASTM D 955
2.54 mm

横向(Across Flow)

0.8 % ASTM D 955
2.54 mm

磨耗

7 mg/1000cy ASTM D 3489
H-18, 1,000-g Load
机械性能 值/单位 测试标准 测试条件

拉伸强度

100%延伸率时

3.4 Mpa ASTM D 412

300%延伸率时

5.2 Mpa ASTM D 412

-

25.5 Mpa ASTM D 412

拉伸延伸率

断裂(brk)

770 % ASTM D 412

弯曲模量

106.9 Mpa ASTM D790
-22°F (-30°C)

弯曲模量

14.5 Mpa ASTM D790
73°F (23°C)

撕裂强度

60.5 kN/m ASTM D 624
Die C

压缩永久形变

30 % ASTM D 395
22 Hours at 158°F (70°C)

压缩永久形变

11 % ASTM D 395
22 Hours at 73°F (23°C)

回弹性

68 % ASTM D 2632
硬度性能 值/单位 测试标准 测试条件

邵氏硬度 A

70 A ASTM D 2240
热学性能 值/单位 测试标准 测试条件

维卡软化温度(Vicat)

75 °C ASTM D1525
Rate A (50°C/h), Loading 1 (10 N)

玻璃化温度(Tg)

-57 °C Internal
上一篇:Estane® S175A TPU
下一篇:RTP 2303 A FR
Copyright © 2017-2024 全球材料网 All Rights Reserved.   备案号:苏ICP备2022042014号    网站建设  跨境电商