原厂资料 | 物性表(英文) | |||
产品特性 | 阻燃无卤抗菌防微生物耐水解 | |||
成型方式 | 注塑挤出型材挤出管材挤出线缆挤出 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
密度 | 1.16 g/cm³ | ISO 1183 | |
密度 | 1.16 g/cm³ | ASTM D792 | |
熔体体积流动速率(MVR) | |||
190℃/21.6 kg | 110 cm³/10 min | Internal | |
收缩率 | |||
- | 1 % | Internal | |
磨耗 | 39.3 mm³ | ISO 4649 | |
磨耗 | 40 mm³ | ISO 4649 | |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
100%延伸率时 | 5.79 Mpa | ASTM D 412 | |
100%延伸率时 | 5.2 Mpa | DIN 53504 | |
300%延伸率时 | 9.65 Mpa | ASTM D 412 | |
300%延伸率时 | 8 Mpa | DIN 53504 | |
- | 27.6 Mpa | ASTM D 412 | |
- | 30 Mpa | DIN 53504 | |
拉伸延伸率 | |||
断裂(brk) | 800 % | ASTM D 412 | |
断裂(brk) | 800 % | DIN 53504 | |
撕裂强度 | 40 N/mm | ISO 34 | |
撕裂强度 | 71.8 N/mm | ASTM D 624 | |
压缩永久形变 | 20 % | ASTM D 395 | 24 hrs@23℃ |
压缩永久形变 | 40 % | ASTM D 395 | 24 hrs@70℃ |
压缩永久形变 | 20 % | ISO 815 | 24 hrs@23℃ |
压缩永久形变 | 40 % | ISO 815 | 24 hrs@70℃ |
硬度性能 | 值/单位 | 测试标准 | 测试条件 |
邵氏硬度 A | 82 A | ASTM D 2240 | |
邵氏硬度 A | 82 A | ISO 868 | |
邵氏硬度 D | 30 D | ISO 868 | |
邵氏硬度 D | 30 D | ASTM D 2240 | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热机械分析(TMA) | 190 °C | Internal | TMA High |
热机械分析(TMA) | 165 °C | Internal | TMA Low |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | |||
V-0 | - mm | UL94 |