CoolPoly E-series Thermally Conductive Plastics exhibit electrical conductivity in addition to their thermal conductivity. The electrical conductivity measured as electrical resistivity is commonly in the range 0.1 to 10,000 ohm-cm. This conductivity range is appropriate for shielding electromagnetic and radio frequency energy. CoolPoly E-Series plastics can also be modified to achieve lower levels of electrical conductivity for applications requiring electrostatic dissipation (106 to 1010 ohm-cm). For comparison purposes, unmodified plastics are good electrical insulators (1012 to 1016 ohm-cm) and metals are good electrical conductors (10-6 to 10-1 ohm-cm). 

基本信息
原厂资料
物性表(英文)
产品特性
导热
导电
技术参数
物理性能 值/单位 测试标准 测试条件

密度

1.7 g/cm³ ISO 1183
机械性能 值/单位 测试标准 测试条件

拉伸强度

断裂(brk)

160 Mpa ISO 527-2/1A
5mm/min

拉伸延伸率

断裂(brk)

1.3 % ISO 527-2/1A
5mm/min

弯曲强度

-

250 Mpa ISO 178
23°C

弯曲模量

16000 Mpa ISO 178
23°C

拉伸模量

17300 Mpa ISO 527-2/1A
冲击性能 值/单位 测试标准 测试条件

简支梁缺口(Charpy Notched)

23℃ (73℉)

5.15 kJ/m² ISO 179/1eA

简支梁无缺口(Charpy Unnotched)

23℃ (73℉)

28 kJ/m² ISO 179/1eU
热学性能 值/单位 测试标准 测试条件

比热容

1000 J/kg-K ASTM E 1461

导热系数

1.1 W/(m K) ASTM E 1461
flow

导热系数

0.8 W/(m K) ASTM E 1461
thruplane
电学性能 值/单位 测试标准 测试条件

体积电阻率

6.5E+12 Ohm-m IEC 60093

表面电阻率

1.3E+12 Ohm IEC 60093