Polypropylene 7232 offers excellent impact strength, clarity and gloss. The outstanding parison strength of 7232 allows for large container sizes and higher blow up ratios. 


High Purity: 7232 features minimum taste and odor and optimum thermal stability for superior color and processability. 


FDA: 7232 complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging. 


Recommended Applications: 7232 is ideal for both injection and extrusion blow molded containers for food, drug, cosmetic and toiletry applications requiring superior impact, strength and clarity. 


Processing: 7232 resin processes on conventional blow molding equipment with typical melt temperatures of 390°F-450°F (177°C-232°C).

基本信息
原厂资料
物性表(英文)
产品特性
高光泽
易成型
低气味
食品接触级
法规认证
FDA(食品药品监督管理局)
成型方式
注塑
挤出吹塑
技术参数
物理性能 值/单位 测试标准 测试条件

密度

0.9 g/cm³ ASTM D 1505

熔体质量流动速率(MFR)

-

1.5 g/10min ASTM D1238

收缩率

-

1~2.5 % ASTM D 955
机械性能 值/单位 测试标准 测试条件

拉伸强度

-

23 Mpa ASTM D 638

拉伸延伸率

-

11 % ASTM D 638

弯曲模量

689 Mpa ASTM D790

拉伸模量

827 Mpa ASTM D638
冲击性能 值/单位 测试标准 测试条件

悬臂梁缺口(Izod Notched)

23℃ (73℉)

75 J/m ASTM D256
热学性能 值/单位 测试标准 测试条件

热变形温度(HDT)

0.45 Mpa (66 psi)(4.6kg/cm²)

82 °C ASTM D648

熔融温度(Tm)

143 °C DSC
薄膜性能 值/单位 测试标准 测试条件

水蒸气渗透系数

0.6 g/100in²/day ASTM E96
37.8°C

氧渗透

240 cc/100in²/day ASTM D 1434
23°C

原材料现货供应:133-8218-6680(微信同号)