基本信息
原厂资料 | 物性表(英文) | |||
产品特性 | 高刚性中粘度 | |||
法规认证 | FDA(食品药品监督管理局) | |||
成型方式 | 注塑 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
密度 | 0.9 g/cm³ | ASTM D792 | |
熔体质量流动速率(MFR) | |||
- | 9 g/10min | ASTM D1238 | |
收缩率 | |||
纵向(Flow) | 1.5 % | Internal | 2.00 mm |
横向(Across Flow) | 1.5 % | Internal | 2.00 mm |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
屈服(yld) | 28.5 Mpa | ASTM D638 | |
断裂(brk) | 23.5 Mpa | ASTM D638 | |
拉伸延伸率 | |||
断裂(brk) | 400 % | ASTM D638 | |
弯曲模量 | 1170 Mpa | ASTM D790 | |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
悬臂梁缺口(Izod Notched) | |||
-20℃ (-4℉) | 40 J/m | ASTM D256 | |
23℃ (73℉) | 80 J/m | ASTM D256 | |
硬度性能 | 值/单位 | 测试标准 | 测试条件 |
洛氏硬度R | 95 R | ASTM D785 | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | 121 °C | ASTM D648 | |
相对温度指数(RTI) | |||
冲击w/impact,- | 120 °C | UL 746B | |
电气Elec,- | 120 °C | UL 746B | |
强度w/o impact,- | 120 °C | UL 746B | |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | |||
HB | - mm | UL94 |