Hostacom ERC 487N G22957
PP(聚丙烯)
利安德巴塞尔(LyondellBasell)
产品描述
Hostacom ERC 487N G22957 is a 5% talc filled PP copolymer, with excellent flowability, high stiffness, high dimensional stability and excellent scratch resistance. . It has been designed using the latest advancements in resin synthesis and compounding technology.
This product is also available in other colors, new colors can be developed depending on customer requirements.
This grade is not intended for medical, pharmaceutical, food and drinking water applications.
基本信息
原厂资料 | 物性表-ISO(英文) | |||
产品特性 | 良好的刚性耐刮擦尺寸稳定高流动共聚物低密度填充增强 | |||
颜色形状 | 粒状可定制色 | |||
成型方式 | 注塑 | |||
增强填充 | 5% 滑石粉 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
密度 | 0.95 g/cm³ | ISO 1183 | 23°C |
熔体质量流动速率(MFR) | |||
230°C/2.16 kg | 20 g/10min | ISO 1133 | |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
屈服(yld) | 25 Mpa | ISO 527-1/-2 | 23°C |
弯曲模量 | 1800 Mpa | ISO 178 | 23 °C, Tech. A |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
悬臂梁缺口(Izod Notched) | |||
-40℃ (-40℉) | 2 kJ/m² | ISO 180/1A | |
23℃ (73℉) | 5 kJ/m² | ISO 180/1A | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | 101 °C | ISO 75-1/-2 | Unannealed |