Plexiglas® SG10
PMMA(亚克力)
阿科玛Altuglas (Arkema)
产品描述
Plexiglas® SG10 is an impact modified acrylic resin suitable for injection molding and extrusion. This grade is formulated for approved medical applications. It is a high flow resin designed to provide outstanding light transmission and water white clarity for disposable medical applications.
Some of the features and benefits of Plexiglas® SG10 are:
Chemical Resistance
Good resistance to lipids and drug formulations
Good resistance to isopropyl alcohol (IPA)
Property retention after exposure to hospital antiseptics, acids and bases
Sterilization
Stable to gamma radiation, E-beam, and ETO
Rapid recovery with excellent color stability
Retention of transparency and clarity
Retention of mechanical properties
Durability and Processability
Moldflow simulation data available
Excellent melt processability
Reduced cycle times
Suitable for thin-wall applications and complex multi-cavity molds
Good bondability using solvent, ultrasonic, or radio frequency methods
基本信息
原厂资料 | 物性表-ASTM(英文) 宣传册 (英文) | |||
产品特性 | 透光颜色稳定/易着色易成型短周期成型良好粘合性易焊接无双酚A(BPA)医疗级生物相容电子束灭菌耐伽马射线环氧乙烷灭菌(EtO)耐化学性耐酸耐碱耐脂(肪)高流动 | |||
添加助剂 | 抗冲击剂 | |||
法规认证 | ISO10993(生物相容性)USP Class VI(美国药典) | |||
颜色形状 | 粒状透明 | |||
成型方式 | 注塑挤出 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
比重 | 1.15 - | ASTM D792 | |
熔体质量流动速率(MFR) | |||
230°C/3.8 kg | 3.3 g/10 min | ASTM D 1238 | |
收缩率 | |||
- | 0.3~0.8 % | ASTM D 955 | |
吸水率 | 0.4 % | ASTM D570 | 24 hr immersion |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
断裂(brk) | 36.5 Mpa | ASTM D638 | |
拉伸延伸率 | |||
断裂(brk) | 50 % | ASTM D638 | |
弯曲强度 | |||
断裂(brk) | 71 Mpa | ASTM D790 | |
弯曲模量 | 1860 Mpa | ASTM D790 | |
拉伸模量 | 1860 Mpa | ASTM D638 | |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
悬臂梁缺口(Izod Notched) | |||
23℃ (73℉) | 48 J/m | ASTM D256 | |
硬度性能 | 值/单位 | 测试标准 | 测试条件 |
洛氏硬度 M | 38 M | ASTM D 785 | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | 87.8 °C | ASTM D648 | annealed |
1.8 Mpa (264 psi)(18.6kg/cm²) | 82.8 °C | ASTM D648 | annealed |
维卡软化温度(Vicat) | 93 °C | ASTM D1525 | 50°C/hr; 10N |
维卡软化温度(Vicat) | 80 °C | ASTM D1525 | 50°C/hr; 50N |
导热系数 | 0.22 W/(m K) | ASTM C 177 | |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | |||
HB | - mm | ASTM D 635 | |
光学性能 | 值/单位 | 测试标准 | 测试条件 |
透光率 | 90 % | ASTM D1003 | 3.2 mm |
雾度 | 2 % | ASTM D1003 | 3.2 mm |
折射率 | 1.49 - | ASTM D542 | Nd @ 72°F |
原材料现货供应: