LNP™ LUBRILOY™ D2000P
PC(聚碳酸酯)
沙特基础 (SABIC)
产品描述
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant.
基本信息
原厂资料 | 物性表(英文) | |||
产品特性 | 耐磨易成型 | |||
添加助剂 | 润滑剂 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
密度 | 1.17 g/cm³ | ISO 1183 | |
密度 | 1.17 g/cm³ | ASTM D792 | |
收缩率 | |||
纵向(Flow) | 0.84 % | ISO 294 | flow, 24 hrs |
纵向(Flow) | 0.8 % | ASTM D 955 | flow, 24 hrs |
横向(Across Flow) | 0.8 % | ASTM D 955 | xflow, 24 hrs |
横向(Across Flow) | 0.81 % | ISO 294 | xflow, 24 hrs |
吸湿率 | 0.21 % | ISO 62 | 23°C / 50% RH |
吸湿率 | 0.13 % | ASTM D 570 | 50% RH, 24 hrs |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
屈服(yld) | 56 Mpa | ASTM D638 | |
屈服(yld) | 54 Mpa | ISO 527 | |
断裂(brk) | 46 Mpa | ISO 527 | |
断裂(brk) | 46 Mpa | ASTM D638 | |
拉伸延伸率 | |||
屈服(yld) | 5.9 % | ASTM D638 | |
屈服(yld) | 5.3 % | ISO 527 | |
断裂(brk) | 42.3 % | ASTM D638 | |
断裂(brk) | 43.1 % | ISO 527 | |
弯曲强度 | |||
- | 86 Mpa | ASTM D790 | |
- | 86 Mpa | ISO 178 | |
弯曲模量 | 2270 Mpa | ASTM D790 | |
弯曲模量 | 2300 Mpa | ISO 178 | |
拉伸模量 | 1930 Mpa | ASTM D638 | 50 mm/min |
拉伸模量 | 2100 Mpa | ISO 527 | 1 mm/min |
摩擦系数 | 0.19 - | ASTM D 3702 | Dynamic COF |
摩擦系数 | 0.15 - | ASTM D 3702 | Static COF |
磨损因数 | 44 E-10 in5·min/ft·lb·hr | ASTM D 3702 | |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
悬臂梁缺口(Izod Notched) | |||
23℃ (73℉) | 453 J/m | ASTM D256 | |
23℃ (73℉) | 12 kJ/m² | ISO 180/1A | 80*10*4 |
悬臂梁无缺口(Izod Unnotched) | |||
23℃ (73℉) | NB J/m | ASTM D4812 | |
23℃ (73℉) | 137 kJ/m² | ISO 180/1U | 80*10*4 |
仪器化落镖冲击能量 | |||
23℃ (73℉)峰值 | 40 J | ASTM D3763 | |
多轴冲击 | 43 J | ISO 6603 | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | 137 °C | ASTM D648 | 3.2 mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm²) | 125 °C | ASTM D648 | 3.2 mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm²) | 131 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
线性膨胀系数(CLTE) | |||
纵向(Flow) | 71.2 E-6/°C | ASTM E831 | -40°C to 40°C, flow |
纵向(Flow) | 71.2 E-6/°C | ISO 11359-2 | -40°C to 40°C, flow |
横向(Across Flow) | 72.7 E-6/°C | ASTM E831 | -40°C to 40°C, xflow |
横向(Across Flow) | 72.8 E-6/°C | ISO 11359-2 | -40°C to 40°C, xflow |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | |||
HB | 1.5 mm | UL94 |
原材料现货供应:133-8218-6680(微信同号)