AKROMID® B25 GF 60 LA black (8494)
AKROMID® B25 GF 60 LA black (8494)
PA6
安科罗/开德阜(AKRO-PLASTIC)
产品描述
AKROMID® B25 GF 60 LA black (8494) is a 60% glass fiber reinforced, laser markable polyamide 6. It is characterised by an improved flowability compared to a standard PA 6 GF 60. Furthermore, the material impresses with its high stiffness and strength. It is therefore perfectly suitable for technical applications in industrial engineering and in the automotive industry.
基本信息
原厂资料 | 物性表(英文) |
产品特性 | 高强度高刚性印刷/标记良好流动性填充增强 |
颜色形状 | 粒状黑色 |
成型方式 | 注塑 |
增强填充 | 60% 玻纤 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
密度 | 1.7 g/cm³
| ISO 1183 | 23°C |
收缩率 | | | |
纵向(Flow) |
0.1~0.3 % | ISO 294-4 | |
横向(Across Flow) |
0.3~0.5 % | ISO 294-4 | |
吸湿率 | 0.9~1.2 %
| ISO 1110 | 70°C, 62% r.H. |
螺旋流 | 120 mm
| - | 1mm Thickness |
螺旋流 | 420 mm
| - | 2mm Thickness |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | | | |
断裂(brk) |
255 Mpa | ISO 527-2 | Dry, 5 mm/min |
拉伸延伸率 | | | |
断裂(brk) |
2.4 % | ISO 527-2 | Dry, 5 mm/min |
弯曲强度 | | | |
- |
400 Mpa | ISO 178 | Dry, 2 mm/min |
弯曲模量 | 20000 Mpa
| ISO 178 | Dry, 2 mm/min |
拉伸模量 | 21000 Mpa
| ISO 527-2 | Dry, 1 mm/min |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
简支梁缺口(Charpy Notched) | | | |
23℃ (73℉) |
20 kJ/m² | ISO 179-1/1eA | Dry |
简支梁无缺口(Charpy Unnotched) | | | |
23℃ (73℉) |
100 kJ/m² | ISO 179-1/1eU | Dry |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | | | |
0.45 Mpa (66 psi)(4.6kg/cm²) |
220 °C | ISO 75/B | |
1.8 Mpa (264 psi)(18.6kg/cm²) |
220 °C | ISO 75/A | |
8 Mpa (1160 psi)(81.6kg/cm²) |
190 °C | ISO 75/C | |
线性膨胀系数(CLTE) | | | |
纵向(Flow) |
13 E-6/K | ISO 11359-1/-2 | 23°C to 80°C |
横向(Across Flow) |
60 E-6/K | ISO 11359-1/-2 | 23°C to 80°C |
熔融温度(Tm) | 220 °C
| ISO 11357-3 | DSC, 10K/min |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | | | |
HB |
1.6 mm | UL94 | |
电学性能 | 值/单位 | 测试标准 | 测试条件 |
体积电阻率 | 1.0E+13 Ohm-cm
| IEC 60093 | Dry |
体积电阻率 | 1.0E+13 Ohm-cm
| IEC 62631-3-1 | Dry |
表面电阻率 | 1.0E+12 Ohm
| IEC 62631-3-2 | Dry |