MAGNUM™ 3525
ABS
盛禧奥(TRINSEO)
产品描述
MAGNUM™ 3525 is a medium heat ABS. Its inherent low gloss combined with a high flow makes it specifically suitable for unpainted interior automotive applications. MAGNUM™ 3525 can thereby help you to save up to 50% of the part costs. It is globally available, locally produced in major car production regions.
Benefits:
Lot to lot consistency allowing for optimal machine parameters settings from the start
Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints.
Heat stability during wide range of processing temperatures: enhanced part design freedom
High scratch and mar resistance for an improved aesthetic durability of the parts
Easier recyclability of unpainted part
Applications:
Matt/unpainted interior automotive applications
Mid-consoles
Pillars
Door liners
Glove boxes
基本信息
原厂资料 | 物性表-ISO(英文) | |||
产品特性 | 耐热热稳定低光泽低挥发VOC高流动 |
技术参数
物理性能 | 值/单位 | 测试标准 | 测试条件 |
---|---|---|---|
密度 | 1.05 g/cm³ | ISO 1183 | |
熔体质量流动速率(MFR) | |||
220℃/10 kg | 11 g/10 min | ISO 1133 | |
收缩率 | |||
纵向(Flow) | 0.4~0.7 % | ISO 294-4 | |
堆积(视)密度 | 0.65 g/cm³ | ISO 60 | |
机械性能 | 值/单位 | 测试标准 | 测试条件 |
拉伸强度 | |||
屈服(yld) | 44 Mpa | ISO 527 | 3.20 mm,Injection Molded |
屈服(yld) | 43 Mpa | ISO 527-2/50 | 3.20 mm,Injection Molded |
拉伸延伸率 | |||
屈服(yld) | 3.3 % | ISO 527 | 3.20 mm,Injection Molded |
屈服(yld) | 3.3 % | ISO 527-2/50 | 3.20 mm,Injection Molded |
弯曲强度 | |||
- | 65 Mpa | ISO 178 | 3.20 mm,Injection Molded |
弯曲模量 | 2100 Mpa | ISO 178 | 3.20 mm,Injection Molded |
拉伸模量 | 2200 Mpa | ISO 527-2 | 3.20 mm,Injection Molded |
冲击性能 | 值/单位 | 测试标准 | 测试条件 |
简支梁缺口(Charpy Notched) | |||
-30℃ (-22℉) | 11 kJ/m² | ISO 179/1eA | Injection Molded |
-30℃ (-22℉) | 8 kJ/m² | ISO 179/2C | Injection Molded |
23℃ (73℉) | 17 kJ/m² | ISO 179/1eA | Injection Molded |
23℃ (73℉) | 12 kJ/m² | ISO 179/2C | Injection Molded |
悬臂梁缺口(Izod Notched) | |||
-30℃ (-22℉) | 10 kJ/m² | ISO 180/1A | |
23℃ (73℉) | 17 kJ/m² | ISO 180/1A | |
热学性能 | 值/单位 | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
1.8 Mpa (264 psi)(18.6kg/cm²) | 101 °C | ISO 75-2/A | Annealed |
1.8 Mpa (264 psi)(18.6kg/cm²) | 78 °C | ISO 75-2/A | Unannealed |
燃烧性能 | 值/单位 | 测试标准 | 测试条件 |
UL 防火等级 | |||
HB | 1.5 mm | UL94 | |
HB | 3 mm | UL94 | |
燃烧速率 | 60 mm/min | ISO 3795 | 2 mm |